Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate

Product Details
Customization: Available
Standard: DIN, JIS, AISI, ASTM, GB, BS
Technics: Cold Drawn
Still deciding? Get samples of US$ 1.5/kg
Request Sample
Manufacturer/Factory, Trading Company, Group Corporation
Diamond Member Since 2016

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Management System Certification
ISO 9001, ISO 9000, ISO 20000, SA 8000, BS 25999-2, GAP
Export Year
2016-10-21
  • Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate
  • Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate
  • Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate
  • Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate
  • Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate
  • Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate
Find Similar Products

Basic Info.

Model NO.
1.6552 34CrNiMo6
Surface
Black
Alloy
Non-alloy
Special Use
High-strength Steel Plate, Wear Resistant Steel, Silicon Steel, Cold Heading Steel, Free Cutting Steel, Mold Steel
Certification
RoHS, ISO9001, ASTM, JIS, GB, En, Astmb
Form/Shape
Sheet, Plate, Bar, Rod, Tube, Pipe, Strip, Foil an
Payment
T/T 30% Prepayment, 70% Balance Before Delivery
Delivery Time
2-10 Working Days After Getting The Prepayment
Transport Package
Standard Export Packaging
Specification
Dia0.5-200mm*L500-100000mm
Trademark
Taixie
Origin
China
HS Code
7226999090
Production Capacity
10 Tons Per Month

Product Description

1.[ Cold Extrusion  steel 1.6552 34CrNiMo6 bar& rod&pipe&tube&sheet &plate] 
Introduction:


Heat treated :   1222°C - 1297°C 
 
Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV/Ku (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated 2 Brinell hardness (HBW)
923 713 44 24 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
 
Temperature
(°C)
Modulus of elasticity
(GPa)
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and Thermal conductivity
(W/m·°C)
Specific thermal capacity
(J/kg·°C)
Specific electrical resistivity
(Ω mm²/m)
Density
(kg/dm³)
Poisson's coefficient, ν
11 - -     0.23 -  
758 286 - 24.3 312   -  
713 - 13 41.2     433 114



2.[Cold Extrusion   steel 1.6552 34CrNiMo6   bar& rod&pipe&tube&sheet &plate] 
Surface
:


mill finish (not polished)
brushed
mirror  finish 
embossed 
oxidized
cold-rolled
hot-rolled



3.[Cold Extrusion  steel 1.6552 34CrNiMo6 bar& rod& pipe&tube&sheet &plate] 
Chemistry:

 
C Si
Mn
P
S
0.3-0.38 0.4 0.4-0.7 0.035 0.03
Cr
Mo Ni    
1.4-1.7 0.15-0.3 1.4-1.7    
         


6.These  are our warehouses :-

Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate


Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate



Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate




7.These  are packaging  pictures :

Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate


Cold Extrusion Steel 1.6552 34CrNiMo6 Rod & Bar& Pipe&Tube&Sheet &Plate
 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier