• 1.4417 Alloy 1.4417 Nickel Alloy 03cr25ni7mo3wcun Stainless Steel 03cr25ni7mo3wcun Alloy
  • 1.4417 Alloy 1.4417 Nickel Alloy 03cr25ni7mo3wcun Stainless Steel 03cr25ni7mo3wcun Alloy
  • 1.4417 Alloy 1.4417 Nickel Alloy 03cr25ni7mo3wcun Stainless Steel 03cr25ni7mo3wcun Alloy
  • 1.4417 Alloy 1.4417 Nickel Alloy 03cr25ni7mo3wcun Stainless Steel 03cr25ni7mo3wcun Alloy
  • 1.4417 Alloy 1.4417 Nickel Alloy 03cr25ni7mo3wcun Stainless Steel 03cr25ni7mo3wcun Alloy
  • 1.4417 Alloy 1.4417 Nickel Alloy 03cr25ni7mo3wcun Stainless Steel 03cr25ni7mo3wcun Alloy

1.4417 Alloy 1.4417 Nickel Alloy 03cr25ni7mo3wcun Stainless Steel 03cr25ni7mo3wcun Alloy

Type: Stainless Steel Bars
Standard: ASTM
Grade: 400 Series
Certification: ISO
Shape: Round
Technique: Cold Rolled
Samples:
US$ 300/Piece 1 Piece(Min.Order)
| Request Sample
Customization:
Diamond Member Since 2016

Suppliers with verified business licenses

Manufacturer/Factory, Trading Company, Group Corporation

Basic Info.

Model NO.
1.4417 alloy 1.4417 nickel alloy 03cr25ni7mo3wcu
Surface Treatment
Bright
Transport Package
Wooden Box
Specification
din16mm-500mm
Trademark
taixie
Origin
China
HS Code
2901100000
Production Capacity
5ton

Product Description

1.4417 Alloy 1.4417 Nickel Alloy 03cr25ni7mo3wcun Stainless Steel 03cr25ni7mo3wcun Alloy

1.4417 alloy

1.4417 nickel alloy

03cr25ni7mo3wcun stainless steel

03cr25ni7mo3wcun alloy
 

National standard GB-T standard: Digital grade: S22553, new grade: 022Cr25Ni7Mo3WCuN, old grade: one,

 

2, US standard: ASTMA standard: S31260,

 

3, Japanese JIS standard: SUS329J4L TB,

S22553/022cr25ni7mo3wcun_chemical Composition

Carbon C: ≤0.030,

 

Silicon Si: ≤1.00,

 

Manganese Mn: ≤1.50,

 

P: ≤0.030,

 

Sulfur S: ≤0.040,

 

Chromium Cr: 24.00 ~ 26.00,

 

Nickel Ni: 5.50 ~ 7.50,

 

Mo: 2.50~3.50,

 

(9) Nitrogen N: 0.10~0.30,

 

(10) Copper Cu: 0.20~0.80,

 

(11) Other elements: w:0.10~0.50.

 

Third, 022Cr25Ni7Mo3WCuN Physical properties:

 

Density Density (20ºC)/kg/dm3:7.8,

Specific heat capacity (0~100ºC)/kg/(kg.k):0.5,

Thermal conductivity /w/(m.k)500ºC-:25,

Linear expansion coefficient /(10-6/k)0~100ºC:11.5,

Linear expansion coefficient /(10-6/k)0~565ºC:12.7,

Resistivity (20ºC)/(ω.mm2 /m):0.75,

Longitudinal elastic modulus (20ºC) /GPa:228,

Magnetism: Yes.

Tensile strength (RM/MPa) : 640,

Elongation A/% : 25,

022Cr25Ni7Mo3WCuN Heat Treatment:

Hardness HBW≤ : solid solution 227, hardness HRB≤ : 29, heating temperature: 950~1100, heating method: fast cooling.

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now

You Might Also Like

Diamond Member Since 2016

Suppliers with verified business licenses

Manufacturer/Factory, Trading Company, Group Corporation
Management System Certification
ISO 9001, ISO 9000, ISO 20000, SA 8000, BS 25999-2, GAP
Export Year
2016-10-21