Customization: | Available |
---|---|
Type: | Steel Plate |
Standard: | ASTM, AISI, GB, JIS, DIN, BS |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
C(%) | Si(%) | Mn(%) | P(%) | S(%) | Cr(%) | Ni(%) | Mo(%) | W(%) | B(%) | Al(%) | Ti(%) |
---|---|---|---|---|---|---|---|---|---|---|---|
Max 0.10 | Max 1.00 | Max 1.00 | Max 0.035 | Max 0.025 | 10.0-12.5 | 18.0-21.0 | Max 0.30 | Max 0.20 | 0.008-0.02 | Max 0.80 | 2.60-3.20 |
Yield Rp0.2(MPa) |
Tensile Rm(MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
344 (≥) | 859 (≥) | 14 | 21 | 22 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 322 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson's coefficient, ν |
---|---|---|---|---|---|---|---|
34 | - | - | 0.21 | - | |||
475 | 562 | - | 22.3 | 122 | - | ||
738 | - | 44 | 33.2 | 124 | 233 |