The chemical composition of Aluminium / Aluminum 3.0505 alloy is tabulated below.
Element | Content (%) |
---|---|
Aluminium / Aluminum, Al | 99.0 |
Manganese, Mn | 0.55 |
Magnesium, Mg | 0.50 |
The following table shows the physical properties of Aluminium / Aluminum 3.0505 alloy.
Properties | Metric | Imperial |
---|---|---|
Density | 2.6-2.8 g/cm3 | 0.0939- 0.101 lb/in3 |
Melting point | 641°C | 1185°F |
The mechanical properties of Aluminium / Aluminum 3.0505 alloy are outlined in the following table.
Properties | Metric | Imperial |
---|---|---|
Tensile strength | 150 MPa | 21755 psi |
Yield strength | 130 MPa | 18855 psi |
Shear strength | 97 MPa | 14069 psi |
Elastic modulus | 70-80 GPa | 10153-11603 ksi |
Poisson's ratio | 0.33 | 0.33 |
Elongation | 7% | 7% |
The thermal properties of Aluminium / Aluminum 3.0505 alloy are given in the following table.
Properties | Metric | Imperial |
---|---|---|
Thermal conductivity (@25°C/77°F) | 173 W/mK | 1201 BTU in/hr.ft².°F |
Aluminium / Aluminum 3.0505 alloy has average machinability. However, its machinability can be increased in harder tempers than in annealed condition. Oil lubricants are used for machining this alloy.
Aluminium / Aluminum 3.0505 alloy has good forming characteristics. It is suggested that bend radii should be used in one thickness to 2 t range for annealed H12, H14 and H16 tempers. Bend radii of 2 to 7 t should be used for the H18 temper.
Aluminium / Aluminum 3.0505 alloy has good weldability. It can be welded using arc welding method.
Aluminium / Aluminum 3.0505 alloy does not react to heat treatment except during cold working.
Aluminium / Aluminum 3.0505 alloy can be forged at the temperatures ranging from 372 to 510°C (700 to 950°F).
Aluminium / Aluminum 3.0505 alloy can be hot worked at 205 to 372°C (400 to 700°F)
Aluminium / Aluminum 3.0505 alloy has good cold working characteristics in the harder cold worked tempers.
Aluminium / Aluminum 3.0505 alloy is annealed at 344°C (650°F) followed by cooling in air.
Aluminium / Aluminum 3.0505 alloy can be hardened only by cold working in H12, 14, 16, 18 or 25 tempers.
[aluminium alloy A93105 /3.0505/Almn0.5mg0.5 /N31 sheet]