Customization: | Available |
---|---|
Standard: | DIN, JIS, AISI, ASTM, GB, BS |
Technics: | Cold Drawn |
Still deciding? Get samples of $ !
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV/Ku (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
152 (≥) | 275 (≥) | 21 | 14 | 24 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 |
Temperature (°C) |
Modulus of elasticity (GPa) |
Mean coefficient of thermal expansion 10-6/(°C) between 20(°C) and | Thermal conductivity (W/m·°C) |
Specific thermal capacity (J/kg·°C) |
Specific electrical resistivity (Ω mm²/m) |
Density (kg/dm³) |
Poisson's coefficient, ν |
---|---|---|---|---|---|---|---|
12 | - | - | 0.23 | - | |||
999 | 729 | - | 14.3 | 213 | - | ||
356 | - | 32 | 43.2 | 333 | 214 |
mill finish (not polished)
brushed
mirror
embossed
oxidized
cold-rolled
hot-rolled
3.[Constructional steel 23CrMoB33 1.7271 bar& rod] Chemistry:
C ≤ |
Si ≤ |
Mn ≤ |
P ≤ |
S ≤ |
Cr | Ni |
---|---|---|---|---|---|---|
0.20-0.25 | 0.15-0.35 | 0.70-0.90 | 0.035 | 0.035 | 0.70-0.90 | |
Mo | Al | Cu | Nb | Ti | V | Ce |
0.30-0.40 | ||||||
N | Co | Pb | B | Other | ||
0.0008-0.005 |
6.These are our warehouses :